Table 4 Energy spectrum analysis of tailings sand under different acidification and oxidation degree.
From: Micro-structure and morphology of tailings sand under different oxidation and acidification degree
Element | Oxidation degree 0% | Oxidation degree 25% | Oxidation degree 50% | Oxidation degree 75% | Oxidation degree 100% | |||||
|---|---|---|---|---|---|---|---|---|---|---|
Mass ratio | Atomic ratio | Mass ratio | Atomic ratio | Mass ratio | Atomic ratio | Mass ratio | Atomic ratio | Mass ratio | Atomic ratio | |
O | 25.51 | 28.67 | 25.13 | 42.47 | 40.49 | 52.52 | 45.19 | 55.76 | 55.73 | 63.93 |
Si | 3.07 | 2.51 | 5.93 | 5.71 | 15.76 | 11.65 | 33.55 | 21.92 | 44.80 | 31.49 |
AI | 4.00 | 3.07 | 1.94 | 1.95 | 1.19 | 0.87 | 1.15 | 0.91 | 0.41 | 0.28 |
Fe | 28.21 | 10.78 | 21.90 | 10.60 | 5.77 | 2.14 | 1.18 | 0.42 | 1.06 | 0.35 |
Mg | 1.44 | 0.77 | 0.61 | 0.42 | 0.41 | 0.21 | 0.30 | 0.16 | 0.13 | 0.06 |
Ca | 12.40 | 8.40 | 6.20 | 4.20 | 2.60 | 1.40 | 2.30 | 1.20 | 1.90 | 1.00 |
C | 24.01 | 42.64 | 12.16 | 21.01 | 8.66 | 13.23 | 7.14 | 16.08 | 6.65 | 10.92 |
S | 20.93 | 13.93 | 11.8 | 9.95 | 6.33 | 4.10 | 0.32 | 0.2 | 0.32 | 0.2 |