Figure 10
From: Interfacial properties of SiCf/SiC minicomposites with a scheelite coating

Cross-section view of SiCf/CaWO4/SiC minicomposites oxidized at (a) 1000 °C for 50 h, (b) 1100 °C for 10 h, and (c) 1100 °C for 50 h.
From: Interfacial properties of SiCf/SiC minicomposites with a scheelite coating

Cross-section view of SiCf/CaWO4/SiC minicomposites oxidized at (a) 1000 °C for 50 h, (b) 1100 °C for 10 h, and (c) 1100 °C for 50 h.