Table 4 Parameters of the disintegration curve models of loess samples modified with fly ash and mixtures of additives.
From: Study of the disintegration of loess modified with fly ash and Roadyes
Disintegration time (s) | Fly ash content | |||
|---|---|---|---|---|
0 | 10% | 15% | 20% | |
Roadyes content | ||||
0 | 554.00 | 491.86 | 411.27 | 354.15 |
0.5‰ | 1223.50 | 1396.42 | 1946.15 | 958.67 |
2.5‰ | 1352.10 | 1233.08 | 1154.85 | 1432.18 |
5.0‰ | 1321.90 | 858.74 | 1211.79 | 1904.29 |