Figure 7
From: The permeability of shale exposed to supercritical carbon dioxide

(a–e) porosity growth after SC-CO2 treated at different pressures (f) average porosity growth after SC-CO2 treated at different pressures.
From: The permeability of shale exposed to supercritical carbon dioxide

(a–e) porosity growth after SC-CO2 treated at different pressures (f) average porosity growth after SC-CO2 treated at different pressures.