Figure 3

In K-edge XANES spectra for In-doped zirconolite-2M at concentrations x = 0.10 and 0.20, alongside In2O3 and In foil reference compounds.

In K-edge XANES spectra for In-doped zirconolite-2M at concentrations x = 0.10 and 0.20, alongside In2O3 and In foil reference compounds.