Table 4 Degradation of RB at different initial concentrations.

From: One-pot synthesis of CdS/CeO2 heterojunction nanocomposite with tunable bandgap for the enhanced advanced oxidation process

Dye concentration (ppm)

Degradation percentage

k (min−1)

R2

5

94.8

0.05061

0.99461

10

95.0

0.05104

0.99499

50

95.04

0.05113

0.99614

100

95.08

0.05119

0.99637

150

95.12

0.05174

0.99656

160

95.52

0.05257

0.99716

170

96.0

0.05416

0.99776

180

96.34

0.05567

0.99813

190

97.14

0.05824

0.99827

200

96.18

0.05485

0.99833