Figure 16
From: Study on the preparation and mechanical properties of purple ceramics

Raman spectra at the indentation of the ceramic sample sintered at 1400 °C with 3YSZ amount equal to 80%.
From: Study on the preparation and mechanical properties of purple ceramics

Raman spectra at the indentation of the ceramic sample sintered at 1400 °C with 3YSZ amount equal to 80%.