Figure 8
From: Study on the preparation and mechanical properties of purple ceramics

Raman spectra of ceramic samples containing various 3YSZ content and sintered (a) 1500 °C (b) 1450 °C (c) 1400 °C.
From: Study on the preparation and mechanical properties of purple ceramics

Raman spectra of ceramic samples containing various 3YSZ content and sintered (a) 1500 °C (b) 1450 °C (c) 1400 °C.