Figure 9
From: Study on the preparation and mechanical properties of purple ceramics

SEM images of xwt%3YSZ sintered at 1450 °C (a) x = 20, (b) x = 40, (c) x = 60, (d) x = 80.
From: Study on the preparation and mechanical properties of purple ceramics

SEM images of xwt%3YSZ sintered at 1450 °C (a) x = 20, (b) x = 40, (c) x = 60, (d) x = 80.