Table 2 Effect of the percentages of cement and nanocement suspension during various curing times on the elastic modulus.
Specimens | \({E}_{50}\) (Mpa) | ||||||||
|---|---|---|---|---|---|---|---|---|---|
1 day | 7 days | 28 days | 90 days | – | 1 day | 7 days | 28 days | 90 days | |
0% Cement | 2.49 | 0% Nano | 2.49 | ||||||
1% Cement | 5.93 | 14.63 | 32.37 | 26.39 | 1% Nano | 15.34 | 22.23 | 30.15 | 68.08 |
3% Cement | 21.82 | 60.55 | 53.72 | 93.69 | 3% Nano | 29.45 | 65.16 | 92.29 | 118.37 |
5% Cement | 35.25 | 112.07 | 124.88 | 153.17 | 5% Nano | 96.34 | 127.96 | 195.11 | 277.21 |
7% Cement | 91.76 | 157.8 | 191.68 | 353.58 | 7% Nano | 129.25 | 184.87 | 266.48 | 378.79 |