Figure 2 | Scientific Reports

Figure 2

From: Chemical doping to control the in-situ formed doping structure in light-emitting electrochemical cells

Figure 2The alternative text for this image may have been generated using AI.

(a) The PLQY of the (Super Yellow + TMPE-OH + KCF3SO3 + r-BV0) active material as a function of the r-BV0 chemical reductant concentration. The dashed line is a guide to the eye. (b) The current density as a function of the applied voltage for glass/ITO/Al/(Super Yellow + r-BV0)/Ca/Al electron-only devices for different concentrations of the r-BV0 chemical reductant, as specified in the legend. The thickness of the active material is 100 nm.