Table 7 Impact of autoclaving on the dimensions and surface roughness of CO2 laser-engraved micro-channel on B-doped ER-based microfluidic micro-plates.
Parameter | Before autoclaving | After autoclaving |
|---|---|---|
Width (µm) | 96.68 ± 0.68 | 86.94 ± 3.05 |
Depth (µm) | 95.95 ± 3.21 | 92.53 ± 2.24 |
Ra (µm) | 9.83 ± 1.27 | 10.61 ± 0.29 |