Figure 3

TEM micrograph of spherical shaped synthesized SeNPs performed at 10 mM sodium selenate, 1.5% ascorbic acid and coated with gum Arabic (≈ 46.9 nm, including coat).

TEM micrograph of spherical shaped synthesized SeNPs performed at 10 mM sodium selenate, 1.5% ascorbic acid and coated with gum Arabic (≈ 46.9 nm, including coat).