Figure 17

Macrograph of similar welded joints after corrosion immersion test: (a) welded joint of AA 6082 base alloy using ER 5356 filler rod and (b) welded joint of AA 5083 base alloy using ER 5356 filler rod.

Macrograph of similar welded joints after corrosion immersion test: (a) welded joint of AA 6082 base alloy using ER 5356 filler rod and (b) welded joint of AA 5083 base alloy using ER 5356 filler rod.