Table 3 SEM/EDX results: elemental composition at selected positions after 3, 7 and 12 months (wt%).

From: Glass/steel/clay interactions in a simulated radioactive waste geological disposal system

 

GFeC-3 M

GFeC-7 M

GFeC-12 M

Element

Glass (spec1,3,5)

Fe (spec4)

Clay (spec2)

Glass (spec2,3)

Fe (spec1)

Fe edge (spec7,9)

Fe edge* (spec8)

Clay (spec4)

Glass (spec2,3, 4,5)

Fe (spec1,8)

Clay + Fe (spec6)

Fe edge (spec7)

O

44.0 ± 0.8

 

50.2

40.8 ± 4.0

0.4

3.5 ± 3.2

29.1

44.7

44.9 ± 2.0

1.0 ± 1.0

48.0

10.8

Na

4.4 ± 0.5

 

5.7

4.9 ± 0.3

   

2.2

4.3 ± 1.1

 

2.6

0.8

Mg

  

0.4

    

2.0

0.2 ± 0.1

 

2.4

1.0

Al

0.4 ± 0.4

 

11.7

0.1 ± 0.1

 

0.4 ± 0.4

3.7

9.2

0.9 ± 0.2

 

7.9

3.3

Si

27.1 ± 2.2

 

28.5

27.3 ± 6.0

0.1

0.5 ± 0.5

8.3

27.9

27.0 ± 0.8

 

21.5

6.5

K

0.3 ± 0.3

 

2.5

2.5 ± 2.5

  

0.7

4.2

0.4 ± 0.1

 

2.2

1.2

Ca

      

0.9

 

0.4 ± 0.2

 

0.7

1.3

Fe

0.7 ± 0.7

100.0

  

99.4

95.7 ± 4.0

57.3

6.6

0.6 ± 0.1

99.5 ± 0.7

14.2

75.1

Zr

8.3 ± 0.8

  

8.3 ± 1.5

    

9.0 ± 0.8

   

Ba

15.8 ± 0.5

  

16.2 ± 5.9

    

13.1 ± 0.5

 

0.6

 
  1. (*) sign shows that Fe and clay are simultaneously present at the measured position, but no sign of Fe-oxide formation.