Figure 8
From: Ambipolar surface conduction in oxygen sub-stoichiometric molybdenum oxide films

Evolution of the I–V curve during the second thermal cycle while heating up within the ranges (a) 30–200 and (b) 200–400 °C.
From: Ambipolar surface conduction in oxygen sub-stoichiometric molybdenum oxide films

Evolution of the I–V curve during the second thermal cycle while heating up within the ranges (a) 30–200 and (b) 200–400 °C.