Table 1 Sample coding according to CuO@ZnO core/shell NPs concentration and the thickness of the nanocomposite films.
Structure | CMC (g) | CuO (g) | D.W. (mL) | Thickness (mm) |
|---|---|---|---|---|
CMC | 0.250 | 0.000 | 50 | 0.032 |
CS-1 | 0.245 | 0.005 | 0.024 | |
CS-2 | 0.240 | 0.010 | 0.039 |
Structure | CMC (g) | CuO (g) | D.W. (mL) | Thickness (mm) |
|---|---|---|---|---|
CMC | 0.250 | 0.000 | 50 | 0.032 |
CS-1 | 0.245 | 0.005 | 0.024 | |
CS-2 | 0.240 | 0.010 | 0.039 |