Table 3 Energy dispersive X-ray spectroscopy (EDX) analysis of all samples.
From: Facile synthesis of ZnO/Hal nanocomposite for arsenite (As(III)) removal from aqueous media
Sample | Element | Wt% | Atomic % |
|---|---|---|---|
ZnO@Hal | O | 35.65 | 50.86 |
Si | 29.43 | 23.92 | |
Zn | 8.63 | 3.03 | |
Al | 26.24 | 22.19 | |
ZnO/Hal | O | 46.44 | 69.37 |
Si | 12.66 | 10.7 | |
Zn | 31.45 | 11.49 | |
Al | 9.51 | 8.42 |