Table 5 Crystallite width of untreated and heat-treated wood before and after fungal exposure.
Crystallite width (nm) | ||||
|---|---|---|---|---|
Unexposed | Brown-rotted | White-rotted | ||
P. tomentosa | Control | 2.8 ± 0.1 | 2.7 ± 0.1 | 2.6 ± 0.1 |
AHT at 180 °C | 2.7 ± 0.1 | 2.6 ± 0.1 | 2.7 ± 0.1 | |
AHT at 220 °C | 2.9 ± 0.2 | 2.7 ± 0.1 | 2.7 ± 0.1 | |
OHT at 180 °C | 2.7 ± 0.2 | 2.5 ± 0.1 | 2.8 ± 0.1 | |
OHT at 220 °C | 2.7 ± 0.1 | 2.7 ± 0.1 | 2.7 ± 0.1 | |
P. koraiensis | Control | 2.9 ± 0.2 | 2.4 ± 0.3 | 2.5 ± 0.0 |
AHT at 180 °C | 2.8 ± 0.1 | 2.6 ± 0.1 | 2.8 ± 0.1 | |
AHT at 220 °C | 2.8 ± 0.0 | 2.8 ± 0.1 | 2.8 ± 0.1 | |
OHT at 180 °C | 2.9 ± 0.2 | 2.9 ± 0.1 | 2.8 ± 0.1 | |
OHT at 220 °C | 3.1 ± 0.1 | 3.0 ± 0.1 | 3.0 ± 0.1 | |