Table 2 sample type 1 different material compositions extruded using a 1.75 mm nozzle at 60 °C. The sample types were made with the base materials protein (5 g) and water (3 g), while changing the additive materials.
From: Biodegradable suture development-based albumin composites for tissue engineering applications
Sample no | Composite Concentrations | |||
|---|---|---|---|---|
Gelatin | Glycerin | PVA | Hyaluronic acid | |
Sample 1.1 | 2 g | 3 g | 0 | 0 |
Sample 1.2 | 3 g | 2 g | 0 | 0 |
Sample 1.3 | 3 g | 2 g | 2 g | 0 |
Sample 1.4 | 3 g | 2 g | 2 g | 0 |
Sample 1.5 | 3 g | 2 g | 0 | 2 g |