Table 4 Sample Type 2: Different compositions extruded using a 0.9 mm nozzle at 60 °C.Base materials used were protein (5 g), water (3 g), Sodium alginate (0.22 g) and poly lactic acid (PLA) (0.73 g), while the additive materials were changed.

From: Biodegradable suture development-based albumin composites for tissue engineering applications

Sample No

Composite Concentrations

Gelatin

Glycerin

PVA

Hyaluronic acid

Sample 2.1

2 g

3 g

0

0

Sample 2.2

3 g

2 g

0

2 g

Sample 2.3

3 g

2 g

2 g

0

Sample 2.4

3 g

2 g

2 g

2 g