Table 5 Sample type 2: mechanical proprieties of sutures produced from nozzle 0.9 mm.
From: Biodegradable suture development-based albumin composites for tissue engineering applications
Sample 2.1 | Sample 2.2 | Sample 2.3 | Sample 2.4 | |
|---|---|---|---|---|
Elongation % | 14.5 | 11.5 | 36 | 38 |
Max load (N) | 5.044 | 21.223 | 17.001 | 16.993 |
Tensile stress at max load (MPa) | 5.3086 | 7.727 | 6.393 | 9.616 |