Table 2 Orthogonal test analysis and results of Ra and ΔRa.

From: Improvement of roughness in ultrasonic assisted magnetorheological finishing of small titanium alloy nuts by orthogonal test method

Indexes

 

A (n1)

B (n2)

C (Au)

D (I)

Ra

K1

0.145

0.149

0.146

0.125

K2

0.130

0.131

0.128

0.111

K3

0.131

0.127

0.133

0.171

R

0.015

0.021

0.018

0.06

Factor influence sequence

D > B > C > A

ΔRa

G1

87.61

86.50

88.10

89.07

G2

87.75

89.31

88.37

90.08

G3

89.17

88.74

88.08

85.38

R

1.56

2.81

0.29

4.7

Factor influence sequence

D > B > A > C