Table 1 XPS surface elemental composition of synthesized material and XRD peak intensity ratio of g-C3N4 (002) to ZnO (101).

From: Solar-matched S-scheme ZnO/g-C3N4 for visible light-driven paracetamol degradation

 

ZnO

g-C3N4

ZnO/g-C3N4

3%

ZnO/g-C3N4

5%

ZnO/g-C3N4

10%

ZnO/gC3N4

20%

At%: Zn

35.51

39.99

40.22

38.86

34.61

At%: O

45.19

1.85

40.48

38.38

40.35

37.35

At%: C

42.43

15.64

16.83

17.97

20.26

At%: N

55.72

1.37

2.24

2.81

7.78

I(002)/I(101)

0.023

0.038

0.047

0.063