Table 1 Preparation method used for self-wrinkling PUA coatings.

From: Preparation of a self-matting, anti-fingerprint and skin-tactile wood coating via biomimetic self-wrinkling patterns

Coating

LED lamp (mW/cm2)

Excimer lamp (mW/cm2)

UV mercury lamp (mW/cm2)

Coating thickness (μm)

Curing time (s)

LED 0

0

30

300

60

10

LED 200

200

30

300

60

10

LED 500

500

30

300

60

10

LED 800

800

30

300

60

10

LED 1000

1000

30

300

60

10

EX 0

500

0

300

60

10

EX 10

500

10

300

60

10

EX 20

500

20

300

60

10

EX 30

500

30

300

60

10

EX 40

500

40

300

60

10

UV 150

500

30

150

60

10

UV 225

500

30

225

60

10

UV 300

500

30

300

60

10

Control

0

0

300

60

10