Figure 7

Schematic diagram and photograph of the varied channel widths and wall thicknesses (nominal dimensions indicated in mm) and SEM images with the measured dimensions in mm and shrinkage in %. This SS channel was sintered at 1135 °C for 12 h. Scale bar: photograph = 3 mm, SEM images = 0.5 mm.