Table 3 Electrochemical Impedance parameters, double layer capacitance, % Inhibition efficiency and thickness of passive film formed on the surface of rebars embedded in mortars determined after 43 cycles of wet/dry treatments of mortars.
Id of samples | Rs (KΩ cm2) | Rct (KΩ cm2) | Y0 (S·sα/cm2) × 10−6) | Α | Cdi (μFcm−2) | t, nm | %E | Wd, S × s1/2/cm2 × 10−6 | (Χ2) × 10−3 |
|---|---|---|---|---|---|---|---|---|---|
Control | 1.61 | 1.04 | 42.4 | 0.63 | 8.9 | 4.47 | – | 1.9 | 5.8 |
0.10NIS + 0.10 BTAH | 1.22 | 9.34 | 33.0 | 0.58 | 3.25 | 12.26 | 88.8 | 3.2 | 2.7 |
0.15NIS + 0.20 BTAH | 1.19 | 23.25 | 32.3 | 0.63 | 3.13 | 12.73 | 95.5 | 5.4 | 2.9 |
0.15NIS + 0.25 BTAH | 0.89 | 19.22 | 31.7 | 0.55 | 1.69 | 23.57 | 94.6 | 4.0 | 0.25 |