Table 2 Electrospinning parameters.

From: Fabrication and characterization of polyvinyl alcohol-chitosan composite nanofibers for carboxylesterase immobilization to enhance the stability of the enzyme

Parameters

Values

Voltage (kV)

21

Distance between electrodes (cm)

12

Flow rate (mL/h)

0.5

Humidity (%)

35 ± 1

Temperature (°C)

25 ± 1

Needle diameter (mm)

0.8