Fig. 3
From: Investigation on the creep mechanism of PA6 films based on quasi point defect theory

DMA curve of storage modulus, loss modulus and loss factor of PA6 film with temperature (heating rate of 3 °C/min, loading frequency of 1 Hz).
From: Investigation on the creep mechanism of PA6 films based on quasi point defect theory

DMA curve of storage modulus, loss modulus and loss factor of PA6 film with temperature (heating rate of 3 °C/min, loading frequency of 1 Hz).