Table 2 Creep tests at different temperatures with stress of 3 MPa.
From: Investigation on the creep mechanism of PA6 films based on quasi point defect theory
Sample | Thickness (mm) | Stress (MPa) | Temperature (℃) |
|---|---|---|---|
3–30 | 0.26 | 3 | 30 |
3–33 | 0.27 | 3 | 33 |
3–37 | 0.26 | 3 | 37 |
3–40 | 0.25 | 3 | 40 |
3–50 | 0.26 | 3 | 50 |