Fig. 8 | Scientific Reports

Fig. 8

From: Effect of ultrasound on the physicochemical, mechanical and adhesive properties of micro-arc oxidized coatings on Ti13Nb13Zr bio-alloy

Fig. 8

Load results in initial cohesive cracks (Lc1) and critical load causes total damage of the coating (Lc2) values for the MAO and UMAO coatings (n = 3). All samples experience coating delamination, but the force at which the substrate becomes visible varies. All data are expressed as means ± SD. There is no statistically detected difference as compared to the MAO specimen in each group.