Fig. 8
From: Dynamic properties of mortar with oyster shell sand replacement

Development of absorbed energy with strain before failure: (a) pg=0.2 MPa, (b) pg=0.3 MPa, (c) pg=0.4 MPa.
From: Dynamic properties of mortar with oyster shell sand replacement

Development of absorbed energy with strain before failure: (a) pg=0.2 MPa, (b) pg=0.3 MPa, (c) pg=0.4 MPa.