Fig. 3

The microstructures of the fractured surfaces of bone cement after 24 h of storage, (A) Simplex P control cement, (B) Simplex P cement exposed to NS (ambient temperature), (C) Simplex P cement exposed to cold NS, and (D) FIX 1 cement exposure to cold NS.