Table 3 Design table of Al7075/WC composite under furnace cooled condition.
Aging condition | Load (N) | Sliding distance (m) | Wear rate (mm/m3) |
|---|---|---|---|
Non-Aged | 10 | 1000 | 0.00754 |
Non-Aged | 20 | 1500 | 0.00972 |
Non-Aged | 30 | 2000 | 0.01174 |
250 °C | 10 | 1500 | 0.00244 |
250 °C | 20 | 2000 | 0.00287 |
250 °C | 30 | 1000 | 0.00269 |
450 °C | 10 | 2000 | 0.00316 |
450 °C | 20 | 1000 | 0.00331 |
450 °C | 30 | 1500 | 0.00343 |