Table 5 ANOVA table of Al7075/WC composite under furnace cooled condition.

From: Experimental investigation of influence of age hardening temperature and cooling medium on tribological behaviour of aluminium/tungsten carbide metal matrix composite

Source

DF

Adj SS

Adj MS

F-value

P-value

Regression

3

0.000079

0.000026

5.66

0.046

Aging condition (°C)

1

0.000072

0.000072

15.36

0.011

Load (N)

1

0.000004

0.000004

0.90

0.386

Sliding distance (m)

1

0.000003

0.000003

0.72

0.436

Error

5

0.000023

0.000005

  

Total

8

0.000103

   

R2- value = 76.86%

Adjusted R2-value = 80.97%