Table 8 ANOVA table of Al7075/WC composite under the atmospheric cooled condition.

From: Experimental investigation of influence of age hardening temperature and cooling medium on tribological behaviour of aluminium/tungsten carbide metal matrix composite

Source

DF

Adj SS

Adj MS

F-value

P-value

Regression

3

0.000035

0.000012

9.02

0.018

Aging Condition (degree)

1

0.000016

0.000016

12.46

0.017

Load (N)

1

0.000006

0.000006

4.65

0.084

Sliding Distance (m)

1

0.000013

0.000013

9.94

0.025

Error

5

0.000006

0.000001

  

Total

8

0.000042

   

R2-value = 95.98%