Fig. 9

Reuse of iron-doped composites in the absence and presence of hydrogen peroxide. Experimental conditions: UVA irradiation, pH of 5.5; CRB5 = 10 mg/L; CMB = 10 mg/L; CH2O2 = 10 mM; reaction time = 2 h; dynamic regime.

Reuse of iron-doped composites in the absence and presence of hydrogen peroxide. Experimental conditions: UVA irradiation, pH of 5.5; CRB5 = 10 mg/L; CMB = 10 mg/L; CH2O2 = 10 mM; reaction time = 2 h; dynamic regime.