Table 5 Examination of mortar variance.

From: Applications of bamboo fiber and bamboo stem ash with styrene butadiene rubber in cement mortar for sustainable structural application

Indexes of performance

Parameter

Degree of freedom

Sum of squares

Mean square

Contribution (%)

Dry density

W/B

3

240,730

80243.4

66.73

BSA (%)

3

30,147

10049.1

8.35

SBR (%)

3

2208

736.1

0.61

BF (%)

3

79,286

26428.7

21.98

Residual

3

8341

2780.4

2.31

Total

15

360,713

120237.7

100

Water absorption

W/B

3

0.6798

0.2266

2.15

BSA (%)

3

3.3721

1.1240

10.71

SBR (%)

3

1.1557

0.3852

3.67

BF (%)

3

25.7121

8.5707

81.67

Residual

3

0.5632

0.1877

1.78

Total

15

31.4829

10.4942

100

Compressive strength

W/B

3

492.02

164.008

54.04

BSA (%)

3

89.56

29.854

9.83

SBR (%)

3

13.96

4.654

1.53

BF (%)

3

234.90

78.301

25.80

Residual

3

79.99

26.662

8.78

Total

15

910.44

303.479

100

Flexural strength

W/B

3

14.2341

4.7447

56.03

BSA (%)

3

2.0362

0.6787

8.01

SBR (%)

3

0.3904

0.1301

1.53

BF (%)

3

6.2324

2.0775

24.53

Residual

3

2.5077

0.8359

9.87

Total

15

25.4008

8.4669

100