Fig. 11

SEM images of surface textures after laser surface texturing with different scanning speeds on stainless steel on copper (Cu, a to d) and the titanium alloy Ti64 (Ti, e to h). λ = 1030 nm, τ = 260 fs, fP = 200 kHz, d0 = 120 ± 5 µm, ϕ0 = 0.65 J/cm2, py = 24 µm, n = 1.