Fig. 4

Effect of the replacement percentages (5%, 10% and 15%) by weight of slag with sodium silicate + sodium carbonate activator on the compressive strength at 28 days.

Effect of the replacement percentages (5%, 10% and 15%) by weight of slag with sodium silicate + sodium carbonate activator on the compressive strength at 28 days.