Table 8 Material removal rate Dm and roughness improvement rate RIR for analysed different metallic and non-metallic tools given in Table 7.
Tool type | dm [mg/min] | RIR [%] |
|---|---|---|
Segmented polyamide disc printed by SLS - under investigation in the article | 33.68 | 75% |
UV-curable resin bond diamond lapping plate32 | 2.03 | 60% |
Conventional disc made of cast iron32 | 3.08 | 55% |
Conventional disc made of cast iron33 | 10.36 | 18% |
Electroplated diamond disc with the nickel plating ratio Tb = 35%5 | 29.06 | 86% |
Electroplated diamond disc with the nickel plating ratio Tb = 50%5 | 35.06 | 36% |
Electroplated diamond disc with the nickel plating ratio Tb = 65%5 | 41.17 | 17% |