Fig. 7


Load–displacement and toughness behavior of the samples under compression containing different PET fiber % at different w/b ratios (a) w/b = 0.35, (b) w/b = 0.40 and (c) w/b = 0.45.


Load–displacement and toughness behavior of the samples under compression containing different PET fiber % at different w/b ratios (a) w/b = 0.35, (b) w/b = 0.40 and (c) w/b = 0.45.