Table 1 Textural properties of prepared samples.
Samples | SBET a (m2/g) | Dpb (nm) | Vp c (cm3/g) |
|---|---|---|---|
Zr-MOF | 1123 | 1.97 | 0.04 |
Zr-MOF-glutaraldehyde | 745 | 1.76 | 0.04 |
Zr-MOF-glutaraldehyde-Adn | 610 | 1.73 | 0.03 |
Zr-MOF-glutaraldehyde-Adn@Fe3O4 | 120 | 1.68 | 0.01 |
Samples | SBET a (m2/g) | Dpb (nm) | Vp c (cm3/g) |
|---|---|---|---|
Zr-MOF | 1123 | 1.97 | 0.04 |
Zr-MOF-glutaraldehyde | 745 | 1.76 | 0.04 |
Zr-MOF-glutaraldehyde-Adn | 610 | 1.73 | 0.03 |
Zr-MOF-glutaraldehyde-Adn@Fe3O4 | 120 | 1.68 | 0.01 |