Table 4 Normal distribution coefficient of compressive strength of FNS-GC.
From: Performance and statistical characteristics of ferronickel slag geopolymer concrete
FNS replacement rate | μ1 | s1 | Effect size D | p-value | Result |
|---|---|---|---|---|---|
0 | 1.0139 | 0.1041 | 0.097 | 0.961 | Not reject |
33% | 1.0656 | 0.1675 | 0.130 | 0.763 | Not reject |
66% | 0.9753 | 0.0937 | 0.068 | 1.000 | Not reject |
100% | 0.9539 | 0.1106 | 0.121 | 0.834 | Not reject |