Fig. 10

Storage modulus E’ and loss factor tan δ as functions of temperature (30–150 °C) of WPS composites filled with different content of SD/CW powder.

Storage modulus E’ and loss factor tan δ as functions of temperature (30–150 °C) of WPS composites filled with different content of SD/CW powder.