Fig. 10 | Scientific Reports

Fig. 10

From: Enhanced structural and electrical properties of furnace-cooled SrZrO3-modified BFBT lead-free piezoceramics for high-temperature applications

Fig. 10The alternative text for this image may have been generated using AI.

Frequency dependence of the real part of impedance (Z′) of furnace-cooled (FC–BFBT–SZx ceramics x = 0, 0.02, and 0.04 mol%) at various temperatures (300–500 ℃), showing the transition from insulating to conductive behavior with increasing frequency.