Table 8 Static Bending strength of thermally modified wood of Salix tetrasperma (kN/mm2).

From: Enhanced strength and chemical stability of Salix tetrasperma wood through thermal modification

Duration(h)

Temperature (°C)

2 h

4 h

6 h

Mean

SD

CV

60 °C

0.011

0.01

0.011

0.011

0.0006

5.4127

80 °C

0.010

0.011

0.009

0.010

0.0010

10.0000

100 °C

0.010

0.009

0.008

0.009

0.0010

11.1111

120 °C

0.010

0.009

0.009

0.009

0.0006

6.1859

140 °C

0.008

0.008

0.007

0.008

0.0006

7.5307

160 °C

0.007

0.008

0.007

0.007

0.0006

7.8730

180 °C

0.007

0.007

0.008

0.007

0.0006

7.8730

200 °C

0.007

0.006

0.006

0.006

0.0006

9.1161

Control

0.012

0.012

0.012

0.012

  

Mean

0.009

0.009

0.009

   

CD0.05

 

Temperature (T)

0.001

Duration (D)

NS

Temperature × Duration (T × D)

NS