Table 5 Microhardness results of Sn-0.7 Cu-x (WS, RHA) composite solders.
Alloy | HV (kg/mm2) | SD |
|---|---|---|
S0 | 13.29 | 0.54 |
S1 | 14.94 | 0.76 |
S2 | 13.63 | 0.47 |
S3 | 18.92 | 0.66 |
S4 | 14.05 | 0.52 |
Alloy | HV (kg/mm2) | SD |
|---|---|---|
S0 | 13.29 | 0.54 |
S1 | 14.94 | 0.76 |
S2 | 13.63 | 0.47 |
S3 | 18.92 | 0.66 |
S4 | 14.05 | 0.52 |