Table 2 Physical characteristics of all utilized geopolymer binders.
From: Integrating quarry dust and industrial waste in producing eco-friendly hybrid geopolymer concrete
Characteristics | CEM I 42.5 N | FA | Slag | GP | BP | DP |
|---|---|---|---|---|---|---|
Specific gravity (g/cm3) | 3.15 | 2.57 | 2.90 | 2.65 | 2.95 | 2.84 |
Specific surface area (cm2 /g) | - | 26,700 | 6000 | 8000 | 5300 | 1700 |
Chloride (Cl) | - | - | 0.30 | 0.11 | - | 1.01 |
Loss of ignition (L.O.I) | 1.70 | 0.20 | - | 0.65 | 1.34 | 44.07 |