Table 3 Taguchi’s design of experiments and effects of HA/ZnO/GO synthesised nanocomposites on the survival rate of S. mutans.

From: Taguchi optimisation of ZnO and GO-integrated HA nanocomposite with improved antibacterial performance

Experiment

HA

(mg/mL)

GO

(mg/mL)

ZnO

(mg/mL)

Bacterial survival

(log₁₀ CFU/mL)

20.08

40.16

80.32

0.01

0.02

0.03

2.44

4.88

7.32

1

 

20.08

  

0.01

  

2.44

 

1.05

2

 

20.08

  

0.02

  

4.88

 

0.78

3

 

20.08

  

0.03

  

7.32

 

0.61

4

 

40.16

  

0.01

  

4.88

 

1.27

5

 

40.16

  

0.02

  

7.32

 

0.94

6

 

40.16

  

0.03

  

2.44

 

1.12

7

 

80.32

  

0.01

  

7.32

 

1.44

8

 

80.32

  

0.02

  

2.44

 

1.63

9

 

80.32

  

0.03

  

4.88

 

0.89